Détails sur le produit:
|
| Type de liaison: | Antioxydant amélioré | Porosité apparente: | 6% |
|---|---|---|---|
| Teneur en MgO: | 73% | Densité apparente: | 3,04 g/cm3 |
| Résistance à l'écrasement du froid: | 41 MPa | Réfractarité sous charge: | 1700°C |
| Contenu en carbone fixe: | 16% | ||
| Mettre en évidence: | C16 Taphole Brick,Antioxidant Enhanced Block,Iron Tapping Refractory |
||
Sintered magnesia and flake graphite form the base of these C16 bricks, and the antioxidant enhanced system locks both phases into a body that keeps its shape through 1730 C service in the blast furnace taphole of a blast furnace iron drain. Each brick is dense enough to limit slag penetration, with 6% apparent porosity and 3.04 g/cm3 bulk density, but still tough enough for blast furnace taphole service where the shell flexes and the lining moves. Cold crushing strength